Flotation of Insoluble Slimes from Potash Ore
Flocculant and collector were gently folded into the pulp with a spatula for a conditioning period of 2 minutes. The deslimed pulp was diluted to 23-percent-solids pulp density in a Fagergren laboratory flotation cell. The pulp was conditioned, for 2 minutes with 150 grams per ton (0.3 pound per ton) of insol slime blinder and for 2 additional ...