A systematic review of sustainable gold extraction from …
Results: 45% of gold extraction with a non-pre-treated sample; 86% after microwave roasting. Case 3 - A bromine-based solution was applied to extract gold from a sulphide gold ore (Sousa et al., 2018). ® Leaching solution: The leaching solution composed by 4.4 g of NaBr, 30 mL of NaOCl, 42 mL of HCl and 28 mL of H2O per 100 …