Preparation of potassium oleate-kaolin/natural rubber …
Then, PO and kaolin were poured into the ball milling tank of the planetary ball mill in a ratio of 2:25 for wet ball milling modification. The ball milling process took about 2 h. The modified PO-kaolin solution was put into a blast drying oven at 60 °C, and the modified PO-kaolin powder was obtained after repeated drying and washing.