Polymers | Free Full-Text | Mechanical, Wear and Thermal
Subsequently, they were compressed at 180 °C and 100 bar for 10 min by means of a hot press machine (DGTS srl, Verduggio, Monza Brianza, Italy), with Teflon release films (thickness: 300 μm) and subsequently water-cooled. ... The presence of graphite ball-milled for 8 h further lowered the torque value to 3.7 Nm (after 15 min of …